The PET injection molding process for bottle preforms combines material preparation, plasticizing, filling, packing, cooling and release. A useful trial controls the condition of the resin as well as the machine settings. Otherwise, a change attributed to the mould may actually reflect a different material history.
This article focuses on trial preparation and process records for bottle-grade PET preforms. PETG and reinforced engineering PET require their own material-specific guidance. It is not a universal temperature or pressure recipe.
Verify drying rather than recording only a setpoint
PET absorbs moisture. Inadequate drying can allow hydrolytic degradation during melt processing, affecting molecular weight and material performance. Alpek Polyester describes this mechanism in its Laser+ C product information.
For the actual grade, obtain the current supplier's drying instructions and the agreed moisture criterion. Record the dryer type, conditions and throughput relevant to the trial. For a desiccant-air system, this includes airflow and dew-point information; other drying technologies need their own controls.
A heater setpoint is not proof that the material reached the required condition. Identify where and how material moisture is checked, and preserve the result with the trial record.
Protect the prepared material on its route to the machine
A trial record should describe what happened between drying and injection. Identify the feed route, any intermediate storage and interruptions that may have changed the material condition.
If material is changed, record the grade and batch. If an approved recycled-content blend is used, record the blend definition as well. The same trade name or colour does not establish an identical incoming material state.
When production stops, follow the resin and equipment suppliers' shutdown and restart instructions. A successful steady-state setup should not be assumed to remain valid after an unrecorded interruption.
Distinguish the temperature setting from heat history
The barrel profile and hot-runner settings are part of the process record, but they do not describe the entire thermal history. Throughput, residence time, interruptions and the actual equipment arrangement also matter.
Rather than raising temperature repeatedly to address an unexplained appearance change, establish the baseline and investigate one defined question at a time. Follow the material supplier's limits and the site's qualified operating procedure.
This is particularly important when a trial compares a new resin or colour with a previously accepted setup. Preserve the conditions for both runs so the samples remain interpretable.
Separate fill-and-pack observations from cooling observations
During filling and packing, retain the actual process information available on the machine. Relate it to cavity-identified samples instead of relying only on the displayed recipe name.
For cooling, record the relevant supply conditions and the point in the run at which samples were collected. If post-mould cooling or a particular take-out arrangement is used, identify it.
A difference seen immediately after release may not tell the same story as a measurement taken after the agreed conditioning period. Define that period before comparing dimensions.
Build a trial record that another shift can use
The objective is to preserve enough information to repeat and assess the run.
| Record group | Information to preserve |
|---|---|
| Material | Grade, batch, colour/additives and approved blend definition |
| Preparation | Dryer method, relevant conditions and material-check results |
| Setup | Machine, mould revision, hot runner and handling arrangement |
| Process | Baseline settings, available actual values and changes made |
| Samples | Cavity, run stage, collection time and conditioning |
| Results | Agreed measurements, appearance checks and any required tests |
For a proposed YUDO or Husky hot-runner configuration, preserve the actual system identification with the setup. Brand familiarity is not enough to reproduce a process on another installation.
Investigate a changed result with matched evidence
Suppose preforms from a later run show a new colour or appearance difference. Begin by checking whether the comparison is valid: same material specification, comparable preparation, same approved tooling revision and documented sampling conditions.
Next, separate evidence by location and time. Does the change occur in all cavities or in identified positions? Did it begin after an interruption or material change? What was adjusted immediately before it appeared?
These questions help structure the investigation; they are not a diagnosis. Avoid treating every cloudy, discoloured or marked preform as evidence of one cause. Any material-property or chemical test required by the application should use an agreed method.
Keep the preform trial connected to bottle validation
An injection trial establishes evidence about the preform under the recorded conditions. In a two-stage bottle project, it does not by itself establish final container performance after reheating and blowing.
Keep the sample identification when preforms move into the next development stage. This allows a downstream result to be traced back to its material and injection run.
For tooling rather than process-control questions, visit our PET preform mould page or read the preform and blow mould comparison. Send your project information with the material and available trial records so the discussion starts from evidence.